000 | 02614naa a2200349 c 4500 | ||
---|---|---|---|
001 | vtls000635326 | ||
003 | RU-ToGU | ||
005 | 20220210171304.0 | ||
007 | cr | | ||
008 | 181030s2018 ru fs 100 0 rus d | ||
035 | _ato000635326 | ||
040 |
_aRU-ToGU _brus _cRU-ToGU |
||
100 | 1 |
_aИващенко, Яна Олеговна _9487361 |
|
245 | 1 | 0 |
_aВлияние напряжения и длительности микродугового оксидирования на физические характеристики стронций- и кремний-содержащих биопокрытий _cЯ. О. Иващенко, Е. Г. Комарова, Е. А. Казанцева |
246 | 1 | 1 | _aInfluence of micro arc oxidation voltage and duration on physical characteristics of strontium- and silicon-containing biocoatings |
504 | _aБиблиогр.: 3 назв. | ||
520 | 3 | _aThe investigations ofphysical characteristics of Sr- and Si-containing calcium phosphate coatings formed by micro arc oxidation method under different pulsed voltage 200-370 V for various time were performed. The coating thickness grow by exponential law with increasing of the process duration, but the coating roughness and apparent density do not vary, in this case. The increase in the process voltage leads to the linear increase in the coating thickness and roughness from 55 to 150 pm andfrom 3.2 to 8.8 pm, respectively. | |
653 | _aбиопокрытия | ||
653 | _aкальций-фосфатные покрытия | ||
653 | _aстронций | ||
653 | _aкремний | ||
653 | _aмикродуговое оксидирование | ||
653 | _aформирование покрытий | ||
655 | 4 |
_aстатьи в сборниках _9713576 |
|
700 | 1 |
_aКомарова, Екатерина Геннадьевна _9302462 |
|
700 | 1 |
_aКазанцева, Екатерина Александровна _9482623 |
|
773 | 0 |
_tПерспективы развития фундаментальных наук. Т. 1 : сборник научных трудов XV Международной конференции студентов, аспирантов и молодых ученых, 24-27 апреля 2018 г. _dТомск, 2018 _gТ. 1 : Физика. С. 144-146 _z9785946217248 _z9785946217231 _wto000633022 |
|
852 | 4 | _aRU-ToGU | |
856 | 7 | _uhttp://vital.lib.tsu.ru/vital/access/manager/Repository/vtls:000635326 | |
908 | _aстатья | ||
999 | _c441907 |